Treatment and recovery process of marine materials
Boats
In materials such as chromed exterior of the vessel, winches, chain covers, supports, hydrants, windows, pick up lines, down wind, levers, bells, etc.
Treatment
Removing paint, silicones.Stripping of chromium baths, electrolytic baths.
When we pass the piece etched into the bathroom and spent neutralization material refining process as in the old grinding wheel for the material suffer as little as possible, medium grain, fine grain, we turn to the coarse grinding, the pieces, defatted with ultra sound bath, vented disc polished, polished with cotton pad, we went to degreasing and drying.
Treatment of electric bath coating
The pieces were then treated with copper wire tied to his good contacts with current.We spent the electrolytic degreasing bath for the part to be total clean mind fat.
We neutralized the bath.
We went to the bathroom marine copper between 10 minutes and 20 minutes depending on the state of material.
We turn to bright nickel bath.
We return to the copper bath 25 minutes.
We spent the electrolytic degreasing bath.
We turn to bright nickel bath 30 to 45 minutes.
We spent the marine plating bath.
To finish the process we went into the room repolishing.
Then we moved to the packing of the pieces.
Treatment of material inside the vessel
As lamps, cutlery, hand pass, brackets, knobs, handles and faucets sanitary fittings, sculptures, clocks, books and media for all types of parts decoration
Interior treatments are performed in- Gold plated 24 k
- Gold plated 18 k
- Bright Silverplate
- Silverplate mate
Treatment of pieces of bronze, copper and brass
Stripping of previous lacquersDeoxidation
Refined with emery
Coarse grinding and polishing
Repolishing bright
Degreasing of all fats
We painted the deck that can be:
- The coating equipment is electrostatic
- Powder coating equipment
- Baking Equipment